綿その他セルロース繊維の均染性と洗濯堅ろう度に優れた反応染色のための、電解質、固着用アルカリ、封鎖キレート剤、プロセス助剤。
反応染料用助剤とは、セルロース系繊維の反応染色を成立させる染料以外の薬剤であり、染料を繊維に押し込む電解質、それを固着させるアルカリ、そして染浴を清浄かつ均一に保つ工程助剤を指します。 これら自体は色を持ちません。電解質とアルカリの添加量を適切に管理すれば、染色濃度、均染性、洗濯堅ろう度はそれに従います。
Electrolyte forces dye exhaustion onto the fiber. Two salts dominate: sodium sulfate (Glauber's salt) and sodium chloride (common salt). Common salt is cheaper per tonne, but its chloride attacks stainless-steel dyeing machinery over time; sodium sulfate costs more and is gentler on equipment. Choose by total cost, counting machine corrosion, not the salt invoice alone. Typical dosing runs tens of grams per liter, scaled to shade depth.
Alkali triggers the dye-fiber bond. Soda ash (sodium carbonate) is the standard fixation alkali; sodium bicarbonate gives slower, more controlled fixation for difficult shades. Hard-water metal ions cause shade variation and dye aggregation, so a chelant such as EDTA sequesters calcium, magnesium, and iron in the bath. Urea aids dye solubility and fiber swelling, and acetic acid neutralizes the bath before unloading. Soften the water first; it is the cheapest fix for off-shade lots.
当社は、分析および当サイトの改善のため、また — お客様の同意がある場合には — マーケティングおよびB2B訪問者の識別のために、Cookieおよび類似技術を使用します。許可する範囲をお選びください。詳細は プライバシーポリシー.